Quantity / Length in meters: | 1 kg |
---|---|
Contents of packaging: | 500 g Komp. A + 500 g Komp. B |
Gefahrenhinweise: | H373 |
ADDV-42 is a pourable, addition-curing 2-component RTV silicone rubber particularly suitable for the reproduction of models with undercuts using polyurethane and epoxy resins.
As both component batches are matches to each other, we only supply complete batches. It is not possible to obtain individual deliveries of silicone and catalyst.
Technical data:
Color:
Component A: Translucent
Component B: Red
No heat of reaction occurs during vulcanization, so that even larger quantities (e.g. 10 kg) can be poured without the risk of overheating.
If heat is added during curing (e.g. in a heating cabinet or oven), the vulcanization time is reduced by half at a temperature increase of each 10 °C. Heat thus accelerates the cross-linking reaction. The maximum recommended curing temperature is 70 °C.
Caution:
Cannot be processed with our Universal Colour Pastes.
We recommend a test by pouring the mixture of the two components into a limited area of the mould.
The vulcanisation interfering substances (see R&G eWiki) can be on surfaces and also in the ambient air, so it is important to use non contaminated tools and equipment, which were not in contact with them.
As both component batches are matches to each other, we only supply complete batches. It is not possible to obtain individual deliveries of silicone and catalyst.
- Superior flowability
- Fast, shrinkage-free vulcanisation at room temperature
- Good tear strength and tear propagation strength
Technical data:
- Mixing ratio: 1 : 1 component A : component B
- Processing time (at 25 °C): 30-50 minutes
- Demouldable (at 25 °C): After 4-5 hours
- Mixing viscosity: 5.800 ± 500 mPa·s
- Shore A hardness: 40 ± 2
- Tensile strength: >=6.8 N/mm²
- Elongation at break: >= 400 %
- Tear resistance: > 12.5 N/mm
- Linear shrinkage after 7 days at 23 °C: <= 0.1 %
Color:
Component A: Translucent
Component B: Red
No heat of reaction occurs during vulcanization, so that even larger quantities (e.g. 10 kg) can be poured without the risk of overheating.
If heat is added during curing (e.g. in a heating cabinet or oven), the vulcanization time is reduced by half at a temperature increase of each 10 °C. Heat thus accelerates the cross-linking reaction. The maximum recommended curing temperature is 70 °C.
Caution:
Cannot be processed with our Universal Colour Pastes.
We recommend a test by pouring the mixture of the two components into a limited area of the mould.
The vulcanisation interfering substances (see R&G eWiki) can be on surfaces and also in the ambient air, so it is important to use non contaminated tools and equipment, which were not in contact with them.
R&G
R&G Siliconerubber ADDV-42, pack/ 1kg
Product number:
9779932
Manufacturer number:
4152152
Additionally selected items:
Quantity / Length in meters: | 1 kg |
---|---|
Contents of packaging: | 500 g Komp. A + 500 g Komp. B |
Gefahrenhinweise: | H373 |
ADDV-42 is a pourable, addition-curing 2-component RTV silicone rubber particularly suitable for the reproduction of models with undercuts using polyurethane and epoxy resins.
As both component batches are matches to each other, we only supply complete batches. It is not possible to obtain individual deliveries of silicone and catalyst.
Technical data:
Color:
Component A: Translucent
Component B: Red
No heat of reaction occurs during vulcanization, so that even larger quantities (e.g. 10 kg) can be poured without the risk of overheating.
If heat is added during curing (e.g. in a heating cabinet or oven), the vulcanization time is reduced by half at a temperature increase of each 10 °C. Heat thus accelerates the cross-linking reaction. The maximum recommended curing temperature is 70 °C.
Caution:
Cannot be processed with our Universal Colour Pastes.
We recommend a test by pouring the mixture of the two components into a limited area of the mould.
The vulcanisation interfering substances (see R&G eWiki) can be on surfaces and also in the ambient air, so it is important to use non contaminated tools and equipment, which were not in contact with them.
As both component batches are matches to each other, we only supply complete batches. It is not possible to obtain individual deliveries of silicone and catalyst.
- Superior flowability
- Fast, shrinkage-free vulcanisation at room temperature
- Good tear strength and tear propagation strength
Technical data:
- Mixing ratio: 1 : 1 component A : component B
- Processing time (at 25 °C): 30-50 minutes
- Demouldable (at 25 °C): After 4-5 hours
- Mixing viscosity: 5.800 ± 500 mPa·s
- Shore A hardness: 40 ± 2
- Tensile strength: >=6.8 N/mm²
- Elongation at break: >= 400 %
- Tear resistance: > 12.5 N/mm
- Linear shrinkage after 7 days at 23 °C: <= 0.1 %
Color:
Component A: Translucent
Component B: Red
No heat of reaction occurs during vulcanization, so that even larger quantities (e.g. 10 kg) can be poured without the risk of overheating.
If heat is added during curing (e.g. in a heating cabinet or oven), the vulcanization time is reduced by half at a temperature increase of each 10 °C. Heat thus accelerates the cross-linking reaction. The maximum recommended curing temperature is 70 °C.
Caution:
Cannot be processed with our Universal Colour Pastes.
We recommend a test by pouring the mixture of the two components into a limited area of the mould.
The vulcanisation interfering substances (see R&G eWiki) can be on surfaces and also in the ambient air, so it is important to use non contaminated tools and equipment, which were not in contact with them.